ACUAVED Special coating for casting on Chrome-Cobalt.

The coating contains quartz powder.

Do not inhale this powder!

 

The Acuavest® coating is designed to be used with water.

The expansion liquid expansor expansion is appropriate when making the employer. Do not use crystallized exploring liquid!

  • Duplicate model: for 200 g of powder, use the following mixture: 13-14 ml Expansor + 13-14 ml of distilled water.
  • Cylinder: for 400 g of powder, use the following mixture: 55-60 ml of distilled water.
  • In both cases, if the mixture of the coating is done manually, do it on a vibrator.
  • Prepare the liquid according to the desired concentration, add the powder to the liquid and vigorously mix 60 s. Mechanical mixture under vacuum, for 30 s.

 

ACUAVE - working time 4 to 5 minutes at room temperature, powder, liquid and utensils at 20 - 22 ° C.

When liquids or gelatins are colder, the plug is extended.

  • The filling of the models must be carried out on a vibrator.
  • To guarantee smooth and hard surfaces, keep the vibrations for 2 minutes.
  • Duplicate can be performed with gelatin or silicone.
  • Taking time: 30-35 minutes, both for duplicate models and for cylinders.
  • Dehydration of models 40 minutes in an oven at 220-240 ° C.
  • We recommend the technodur hardener.
  • With silicone duplication, this operation is not useful.
  • Put the model of a fine coating or treat it with an extended agent.
  • Fill the cylinder with a slight vibration. Demolage at 35 minutes.

 

Drying, after 35 minutes of socket, bake the models preferably in a cold oven and now at 240 ° C for 40 minutes.

  • Once the cylinders are dry, program the flow temperature.
  • The maximum recommended temperature is 900 ° C for partial prostheses and 1000 ° for total plates.
  • Maintain this temperature for at least 45 minutes.
  • The best expansion is obtained with a heating at the rate of 5 ° C/minute.

 

Once the maintenance period in the oven has passed, do the casting as usual.

  • After the casting, wait until the Masselotte is redest.
  • Once the cylinders are slightly cooled in the open air, immerse them completely in the water.
  • In this way, demouflage becomes very easy.

 

ACUAVEST® powder Store at 18-25ºC Maintain well closed packaging away from humidity.

This coating is sensitive to humidity, prolonged exposure to air can alter the characteristics of the product.

  • Expansor Store at 18-25ºC, prolonged exposure to a temperature below 5ºC or greater than 35ºC can cause freezing and/or destabilization of the product.
  • Maintain well closed packaging after each use.
  • Prolonged air exposure can cause crystallization.

 

Delivery : Cardboard 18 kg (45 x 400 gr) or cardboard 20 kg (10 x 2000 gr) or liquid.

 

 

 

24/7 customer service

Purchases on this site are BtoB, they are neither taken up nor exchanged except hidden defects. Site for professionals.

Secure payments

100% secure online payments. Funding 12 to 60 months - Paypal - Visa - Amex - Mastercard.

Free delivery

Treatment 1 to 2 working days + delivery for France 1 to 3 days. Free port in Metropolitan France from 195 €.

Warranty 1 to 3 years old

According to the brand, the equipment can be guaranteed up to 3 years. We manage your after -sales service during and after the warranty.