Bonding nobil-metal non-precious ceramic reinforcement or laser sipper.
- 47,95 € 47,95 €
- Unit price
Référence: H00029
Bonding nobil-metal for ceramic reinforcement.
Pink-colored aesthetic powder, recommended for reinforcement in non-precious metals or chilled co-CR laser structures before ceramic mounting.
- Improves the metal-ceramic grip .
- Oxidation masking.
- Contains 5 to 10% titanium oxide.
- Fusion point: 800 ° C.
- Cooking temperature: 980 ° C.
Delivery: Bonding Nobil-Metal For non -precious - 1 pot 6 gr.
Scratching the ceramic reinforcement in a traditional way. Then finish of the reinforcement with tungsten strawberries, pass the strawberry over the entire surface, then sandblasting at 250 µ to 3 bars. No steam
Apply a single and uniform layer, proceed to a vacuum cooking to an initial temperature of 650 ° C, increase by 55 ° C per minute. 980 ° C final temperature without any stabilization.
After cooking, the bonding is light yellow to golden yellow depending on the metal used. After cooling, mounting ceramics in a classic way, the final shade will be warmer thanks to the bonding.
NM Bonding achieves a chemical reaction with non -precious alloy and avoids excessive oxidation of the reinforcement.
The correct use guarantees an excellent grip of ceramics, even on long -range reinforcements, without bubbles or cracks.
Strongly improves ceramic-metal adhesion.
The dark color of the oxides is masked and the ceramic obtains a warmer shade.